Noveon Stat-Rite® X-5111 Static Control Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded or injection molded. Features: - Permanently static dissipative
- Humidity insensitive
- Ultra-Clean: low off-gassing, low ionic contamination
- Colorable
- Durable: Can be used repeatedly.
- No carbon/particulate fillers
Applications: - Cleanroom supplies
- Semiconductor handling
- Electronic component handling
- Disk Packaging
Properties of all Stat-Rite® polymer products in the molten state are adversely affected by moisture. Although Stat-Rite® compounds are dry when packaged, trace amounts of moisture can be absorbed during storage and handling. For best results, always dry the material three to four hours at 70°C (160°F) in a dehumidifying hopper dryer. Data provided by Noveon, Inc.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Surface Resistivity per Square
- Static Decay
- Tribocharge
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Drying Temperature
- Dry Time
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|