Novablend® 4760 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: General purpose, high impact, rigid PVC compound
Material Notes: Clear Pellets Description: Novablend® 4760 is a general purpose, high impact, rigid, PVC, extrusion blow molding compound in pellet form. The formulation is designed to provide good processing characteristics, high impact, and excellent thermal stability. Bottles produced with this compound have high gloss and clarity. Applications: Bottles made with Novablend® 4760 are suitable for a variety of toiletries and cosmetic applications, including shampoo, hair rinses, cream, and other personal care products. It is also suitable for variety of household chemical products including detergents, cleansers, disinfectants, waxes for floors, auto and boats, and many pet products. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|