Novablend® 6601 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: Processes easily with excellent weld line and electrical properties
Material Notes: Novablend® 6601 compound is a high impact, high flow, opaque, injection molding formulation. Novablend® 6601 formulation is designed to process easily with excellent weld line and electrical properties. These compounds can be modified to enhance UV stability for outdoor or interior applications. Raw material appearance is Opaque Pellets. Applications: Novablend® 6601 compound is suitable for a variety of general purpose injection molding applications requiring high impact. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Oxygen Index
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|