Novablend® 6650 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: High impact, excellent outdoor weathering, high gloss, and good processing characteristics.
Material Notes: Opaque Pellets Description: Novablend® 6650 is a rigid PVC injection molding compound. This compound has high impact, excellent outdoor weathering, high gloss, and good processing characteristics. Applications: Novablend® 6650 can be used for outdoor applications such as pipe furniture and fencing. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|