Novablend® 7510 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: General purpose, opaque, rigid profile extrusion compound
Material Notes: Novablend® 7510 is a general purpose, opaque, rigid profile extrusion compound in pellet form. Raw material appearance is Opaque Pellets. Novablend® 7510 can be used in the extrusion of small profiles and sheet. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Process
|
|
|
|
| Property Data |