Novablend® 7511 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: General purpose, opaque, rigid PVC compound
Material Notes: Opaque Pellets Description: Novablend® 7511 is a general purpose, opaque, rigid extrusion compound in pellet form. Applications: Novablend® 7511 can be used in the extrusion of small profiles and sheet. It is designed primarily for the electrical connector market. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Oxygen Index
- Process
|
|
|
|