Novablend® 8889 PVC
Subcategory: Vinyl; Thermoplastic; Polymer
Key Words: Rigid vinyl foam powder blend containing a blowing agent.
Material Notes: Opaque Pellets Description: Novablend® 8889 is a rigid vinyl foam compound in pellet form, containing a blowing agent. Density of foams will vary based on processing conditions. Material can be formulated for interior or exterior applications. Information supplied by the manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melt Temperature
- Process
|
|
|
|
| Property Data |