Custom Resins Nylene® PA6/6 Glass Filled 5125 HS Nylon 6/6
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 66; Nylon 66
Material Notes: 25% Glass Filler Grade; Property data for dry as molded samples.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melting Point
|
|
|
|