Custom Resins Nylene® PA6/6 Impact Modified 4114 HS Nylon 6/6
Subcategory: Nylon; Thermoplastic; Nylon 66
Close Analogs: Data provided by the manufacturer
Key Words: Polyamide 66; Nylon 66
Material Notes: High Impact Grade; Property data for dry as molded samples.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |