Nycoa® 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: NYCOA 5100 HS is an impact modified, heat stabilized Nylon 66 resin used for injection molding. This material is specially formulated to provide improved flexibility and ductility vs standard Nylon 66. NYCOA 5100 HS offers outstanding toughness, exceptional processability, and a greater service life at elevated temperatures than standard grades of Nylon 66. It is available in UV stable, and custom colors grades. It also has excellent chemical resistance to greases, oils, and other hydrocarbons. Typical applications include automotive wiring harnesses, motor component housings, gears, and electrical connectors. Information provided by Nycoa, Inc.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|