Nycoa® 1417 HS Heat Stabilized, Impact Modified Nylon 6 Resin
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: NYCOA 1417 HS is a heat stabilized and impact modified Nylon 6. This medium viscosity resin was developed for injection molding and extrusion processes for applications requiring improved toughness, flexibility, and good heat stability. NYCOA 1417 HS is suitable for a variety of applications including plugs, connectors, fasteners, clips, tool housings, and flexible tubing extrusion. Information provided by Nycoa, Inc.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|