NYCOA 2047 Copolymer Nylon 6/69
Subcategory: Nylon; Thermoplastic; Nylon, Other
Key Words: PA 6/69, Polyamide 6/69, Nylon 6/69
Material Notes: extrusion, high melt viscosity. & strength., low crystallinity Information provided by NYCOA, Inc.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Melting Point
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Drying Temperature
|
|
|
|