Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: thermoset, sheet molding compound, fiber glass, fiberglass, fibreglass, fibre glass, FRP composites
Material Notes: Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for use with strong alkalis. Data provided by the manufacturer, Owens Corning.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Arc Resistance
- Specific Heat Capacity
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|