Owens Corning Glass Fiber Reinforced Polyurethane, Flaked Glass (RRIM), 23 wt.% glass
Subcategory: Polyurethane, TS; Thermoset; Polymer
Key Words: thermoset, fiber glass, fiberglass, fibreglass, fibre glass, FRP composites
Material Notes: Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, and ketones. Data provided by the manufacturer, Owens Corning.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- CTE, linear 68°F
- Flammability, UL94
|
|
|
|