Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass
Subcategory: Polyphenylene Sulfide; Thermoplastic; Polymer
Material Notes: Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owens Corning.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Arc Resistance
- Flammability, UL94
|
|
|
|