MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Omnia Plastica - Omniamid Oil - PA6 G.Oil at 50% RH

 

Subcategory: Nylon; Thermoplastic; Nylon 6

Material Notes:
Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a homogeneous dispersion. This produces a notable improvement in the self-lubrication property as well as the shock resistance. Machining is also much easier.

Features:

  • Self-lubricating: the friction coefficient is the lowest of all the cast nylons.
  • Wear resistance: better than PA6 natural.
  • Tensile stress and compressive strength is like Omniamid G whilst shock resistance is higher, the E-modulus is lower.
  • Machining: excellent on machine tools.
  • Colour: orange and black.
Weak Point:

It is hygroscopic, even if to a lower extent than natural PA6 G. Because of the molecular structure, the large-sized cast pieces have better quality than those of small dimensions.

Application:

  • Mechanical: thanks to its excellent self-lubricating property, high shock resistance and compressive strength, together with the possibility to produce large-sized parts, it is widely used to produce bearings and bushings of large diameters as well as pulleys, wheels and anti-wear guides. Because of its excellent abrasion resistance it is used for gear wheels, guide bearings, bearings, sliding bearings, etc. in the building of parts for construction machines, excavators and earthmovers. In the shipbuilding industry its better weather resistance makes it suitable for rollers, haulage, sliding guides, bearings. In cable-car systems its usage includes pulleys, wheels and sliding blocks.
  • Food contact: it cannot be used in contact with food
  • Electrical: usage in the electrical field is to be avoided as the electrical properties change with the change in moisture content.
  • Chemical: it is resistant to alkali, inorganic compounds and solvents.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Dielectric Constant
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。