Omnia Plastica - Akulon GF - PA6 GF Dry
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitable for gears and mechanical parts where excellent wear resistance is required.Features: - Very high wear resistance: this inherent polyamide feature is further increased by the addition of glass. Akulon GF is one of the best wear resistant plastic materials available.
- High compression strength and tensile stress: the fatigue resistance is excellent as are the general mechanical properties.
- Ageing resistance: weatherproof and good resistance at low temperature
- Black colour.
Weak Point: If used in combination with moving parts, the glass filler causes abrasion of the steel parts in contact with the plastic. Application: - Mechanical: very high compressive strength and wear resistance, in fact one the best of all the engineering plastics. This material is particularly suitable for gears and high performance mechanical components which need to operate in demanding environments, such as on construction equipment or earthmovers, without suffering from excessive wear.
- Food contact: it cannot be used in contact with food.
- Electrical: even though the electrical properties change with the moisture content, this nylon is still used where good mechanical features as well as weatherproof performance are required.
- Chemical: it is resistant to alkali, inorganic compounds and solvents.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell M
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|