MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Omnia Plastica - Polytetrafluoroethylene - PTFE

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Material Notes:
A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.

Features:

  • Chemical: a typical fluoropolymer with very high chemical resistance. Mechanical: the mechanical features such as tensile stress and compressive strength are poor. Notably the bearing strain is very low.
  • Very good resistance to low and high temperatures up to 260° C. as well as to UV rays.
  • Low flammability
  • Low friction coefficient
  • Colour: natural
Weak Point:

Poor mechanical properties. The strain is very high, even simply under the weight of the piece.

Application:

  • Chemical: very high chemical resistance to alkali and acids is the main feature of the fluoropolymers. PTFE is used for parts in the petrochemical and chemical industries.
  • Food contact: physiologically inert it is approved for use in contact with food by some standards, whilst in some countries this use is questioned.
  • Electrical: very good dielectric, self-extinguishing and weather stability properties make it suitable for this field.
  • Mechanical: the low friction coefficient makes it suitable for bearings, provided that they work under low charge.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Water Absorption at Saturation
  • Hardness, Shore D
  • Ball Indentation Hardness
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Compressive Strength
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Coefficient of Friction
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。