Omnia Plastica - Polytetrafluoroethylene - PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes: A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features: - Chemical: a typical fluoropolymer with very high chemical resistance. Mechanical: the mechanical features such as tensile stress and compressive strength are poor. Notably the bearing strain is very low.
- Very good resistance to low and high temperatures up to 260° C. as well as to UV rays.
- Low flammability
- Low friction coefficient
- Colour: natural
Weak Point:Poor mechanical properties. The strain is very high, even simply under the weight of the piece. Application: - Chemical: very high chemical resistance to alkali and acids is the main feature of the fluoropolymers. PTFE is used for parts in the petrochemical and chemical industries.
- Food contact: physiologically inert it is approved for use in contact with food by some standards, whilst in some countries this use is questioned.
- Electrical: very good dielectric, self-extinguishing and weather stability properties make it suitable for this field.
- Mechanical: the low friction coefficient makes it suitable for bearings, provided that they work under low charge.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|