Omnia Plastica - Polyethylene 1000 - PE 1000
Subcategory: Polyethylene; Thermoplastic
Material Notes: Polyethylene with a molecular weight of ± 1000,000 with excellent impact strength. PE 1000 is less rigid and has a higher shock resistance than the low molecular weight polyethylene and it is therefore more suitable for applications subject to continuous shocks.Features: - Shock resistance, good even at low temperatures High chemical resistance typical of the polyolefins
- High abrasion resistance
- Low friction coefficient
- Low specific gravity
- Easy machinability
- Colour: natural
Weak Point:Compared to the engineering plastics it has lower thermal and mechanical properties: tensile stress, flexural and compressive strength, etc. Compared to low molecular weight PE, it is less rigid. Application: - Food contact : physiologically inert, it is approved for food contact by the most important standards. Thanks to this feature, it is widely used for components in food machinery, pumps for liquid food etc.
- Chemical: thanks to the high resistance to acids and alkali it is used for components in the chemical industry
- Electrical: very good dielectric properties, weatherproof
- Mechanical: the low friction coefficient and its non hygroscopicity make it suitable for use as a bearing or mechanical parts with low loads, even when operating in water.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell R
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|