Omnia Plastica - Polyvinylchloride - PVC
Subcategory: Vinyl; Thermoplastic
Material Notes: A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Features: - High chemical resistance
- Higher stiffness compared to polyolefins
- Easy machinability on mechanical tools. It can be hot welded
- Colour: grey, ivory, red
Weak Point:Compared to PP it has lower shock and temperature resistance. The high gravity reduces its cheapness. Application: - Chemical: the main application of PVC is in the chemical industry, thanks to its high resistance to acids and alkali and to its rigidity. It is used for components such as valves, flanges, gears, etc. in the chemical, galvanic and petrochemical industries.
- Food contact: it cannot be used in contact with food.
- Electrical: good dielectric properties and weather resistance make it suitable for these applications.
- Mechanical: it is also used for mechanical components in corrosive environments. Compared to polyolefins, it has a higher tensile stress.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell M
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|