Omnia Plastica - Polycarbonate - PC
Subcategory: Polycarbonate; Thermoplastic
Material Notes: This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does make it suitable for precision parts.Features: - Clear Shock resistance
- Dielectric properties
- Dimensional stability
- Colour: clear
Weak Point:It has no self-lubricating power and it is attacked by oil and grease, therefore it cannot be considered suitable for lubricated moving mechanical parts. Application: - Electrical : good dielectric properties. It is mainly used in this field.
- Chemical: the use of PC in the chemical industry is not ideal, due to the poor resistance to hydrocarbons.
- Food contact: physiologically inert if natural.
- Mechanical: it is used for precision mechanisms when good dimensional stability is required.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell M
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|