Omnia Plastica - Polyphenylenoxide Noryl - PPO m
Subcategory: Polystyrene; Polyphenylene Ether/PPO; Thermoplastic
Material Notes: Noryl is a resin based on polyphenylene oxide, modified with styrene. Its main field of application is the electrical one.Features: - Good electrical properties, even at high frequency
- Dimensional stability, low moisture absorption
- Excellent stability
- Gamma ray resistance
- Colour grey
Weak Point:It has poor mechanical features Application: - Electrical: Used particularly for its electrical properties. Suitable for high frequency insulators and components in the electronic industry.
- Mechanical: It has poor mechanical properties.
- Good gamma ray resistance.
- Food contact: It is not used in contact with food.
- Chemical: The resistance is poor and it is not used for chemical applications.
Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Hardness, Rockwell M
- Ball Indentation Hardness
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Minimum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|