ORBILAN® PE 1000 UHMW-PE
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general machine and plant construction, transport and electroplate techniques, bunker and silo linings to the manufacture of fenders and sluices for hydraulic architecture.Information provided by the manufacturer
| Available Properties |
- Density
- Molecular Weight
- Hardness, Shore D
- Ball Indentation Hardness
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact, Notched
- Coefficient of Friction
- Volume Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Attrition
- Water Absorption
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|