Orbilan RubberLen® 55 HMW-PE, dark blue
Subcategory: Polyethylene; Thermoplastic; MDPE
Material Notes: ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very good vibration damping and noise reduction. These properties are highly regarded for applications in the area of lining.Information provided by the manufacturer
| Available Properties |
- Density
- Water Absorption
- Hardness, Shore D
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |