Ovation Polymers NIMA NH PA66UT Nylon 66
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Polyamide 66 - Ultra Tough, Flame Retarded Non-Hal grade with excellent retention of mechanical properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance. Information provided by Ovation Polymers
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Index of Compound
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|