Ovation Polymers SOFTAPLAS S 75A Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Thermoplastic Elastomer – Low tensile set, hydrolytic Stability and excellent balance of properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance. Information provided by Ovation Polymers
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Elongation at Break
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|