Ovation Polymers Uttap SF 600 Polyethersulfone
Subcategory: Polyethersulfone; Thermoplastic
Material Notes: Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers
| Available Properties |
- Specific Gravity
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
|
|
|
|