Panipol Oy DXH Inherently Conductive Polymer

 

Subcategory: Additive/Filler for Polymer

Material Notes:
Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade are controllable resistance in optimal ESD protection range 10^6 - 10^9 O, low sloughing and limited colorability.

The conductivity of Panipol DXH / matrix polymer blend is tunable for insulators over the whole range of semiconductors. Panipol DXH forms a conductive network structure into matrix polymer instead of acting as a filler. The conductive/dissipative property is permanent and built into the polymer chain.

Panipol DXH has been developed mainly for injection molding applications. Panipol DXH should be used in 8 - 15% ratio with PP Heterophasic copolymer to achieve surface resistance values from 10^6 to 10^10 O, (IEC 61340-5-1). The products made out of Panipol DXH are reusable and recyclable.

Typical applications include injection moulded boxes and bins, etc. giving permanent ESD protection for the various packaging applications.

Typical properties tested from a 12/88 ratio of Panipol DXH/Polypropylene Block copolymer (MFI 3.5)

Information provided by Panipol Oy Ltd

Available Properties
  • Specific Gravity
  • Charpy Impact, Notched
  • Surface Resistance
  • Static Decay
  • Front Barrel Temperature
  • Melt Temperature
  • Mold Temperature
  • Injection Pressure
  • Back Pressure
  • Injection Speed
  • Plasticizing Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。