Panipol Oy T Inherently Conductive Polymer
Subcategory: Additive/Filler for Polymer
Material Notes: Doped polyaniline in tolueneSolution Processing, Coating formulations, Ink formulations Information provided by Panipol Oy Ltd
| Available Properties |
- Solids Content
- Viscosity
- Surface Resistivity per Square
- CAS Number
- Toluene, CAS Number
|
|
|
|