Pau Tai Barium stearate, Monomer Stabilizers
Material Notes: Excellent effect if used with cadmium, zinc, lead. Excellent lubricity and electrical insulation. Resistance to sulfide staining.Applications: Applicable to hard, soft common adhesive plaster, rubber.
| Available Properties |
- Specific Gravity
- Melting Point
- Moisture Content
- Appearance
- Metal Content %
|
|
|
|