Pau Tai UNINOX PA-401, PVC Processing Aid
Material Notes: UNINOX PA-401 is a high molecular weight MMSAN (methyl methacrylate-styrene-acrylonitrile) processing aid. It is a cost effective processing aid for rigid PVC compounds such as calendered sheet, extrusion profile and rigid foam extrusion.Information provided by Pau Tai Industrial Corp. Advantages: - Increases melt strength and elasticity
- Improves thermoforming control
- Reduces PVC fusion time and gate bilsh in injection molding
- Improves rigid PVC foam cell structure
| Available Properties |
- Bulk Density
- Volatiles
- Particle Mesh Size
- Appearance
- Dosage, phr
|
|
|
|
| Property Data |