Permabond Anaerobic Adhesives & Sealants HH131 Threadlocker
Subcategory: Thermoset; Polymer
Material Notes: Permanent, high temp resistant, high strength, up to 1.5" fastenersPermabond`s threadlocking sealants are a cost effective and superior alternative to lock washers and locking metal threaded fasteners. They prevent loosening due to vibration or thermal expansion on all metal threaded fasteners and provide corrosion resistant seals. Information provided by Permabond
| Available Properties |
- Viscosity
- Shear Strength
- Impact Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Max. Gap Fill (mm)
|
|
|
|