Permabond Anaerobic Adhesives & Sealants LM012 Threadsealer
Subcategory: Thermoset; Polymer
Key Words: MIL-S-22473E
Material Notes: No fillers, hydraulic sealingPermabond pipe sealing products are found in various industries including fire protection, HVAC, and plumbing. These PTFE based formulations allow easy assembly and provide an instant seal of 1000 psi. The final cure strength generally exceeds that of most pipe material. The result is a seal which is inert to hydrocarbons, solvents, steam, and glycol-based products. Information provided by Permabond
| Available Properties |
- Viscosity
- Shear Strength
- Impact Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Color
- Max. Gap Fill (mm)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|