Permabond Cyanoacrylate Adhesives 910
Subcategory: Adhesive; Thermoset; Cyanoacrylate
Key Words: A-46060C Type I, Class 2; MIL-A-46050C; MIL-AA-3097
Material Notes: General purpose, metal bondingPermabond`s broad line of cyanoacrylate formulations provides bonding solutions for an ever-increasing scope of applications. Permabond`s complete line includes high performance, rapid cure, high temperature resistant, surface insensitive (for acidic surfaces), and non-blooming/low odor chemistries and can bond everything from plastics, metals and ceramics to wood and composites. Information provided by Permabond
| Available Properties |
- Viscosity
- Shear Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Chemistry
- Color
- Max. Gap Fill (mm)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|