Vyncolit 2530 W Novolac Phenolic
Subcategory: Phenolic; Thermoset; Polymer
Material Notes: Mineral & organic reinforced compound, novolac resin based. Good retention of mechanical properties at high temperature. Information provided by Vyncolit N.V., a Sumitomo Bakelite Company.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|