Perstorp 136 Urea-Formaldehyde w/ cellulose filler
Subcategory: Thermoset; Polymer
Material Notes: A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches. Information provided by Perstorp Compounds Inc.
| Available Properties |
- Linear Mold Shrinkage
- Tensile Strength at Break
- Flexural Strength
- Charpy Impact, Notched
- Surface Resistance
- Dielectric Constant
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Oxygen Index
- Shrinkage
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Injection Pressure
- Hold Pressure
- Back Pressure
- Glow Bar 960°C 180 sec
- Injection speed
- Water Absorption [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|