Perstorp 161 Urea-Formaldehyde w/ cellulose filler
Subcategory: Thermoset; Polymer
Material Notes: Perstorp 161 compression grade has low shrinkage, low water absorption and high strength. It is suitable for circuit breakers and electrical accessories in humid environments. Information provided by Perstorp Compounds Inc.
| Available Properties |
- Linear Mold Shrinkage
- Tensile Strength at Break
- Flexural Strength
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Flammability, UL94
- Oxygen Index
- Shrinkage
- Glow Bar 960°C 180 sec
- Water Absorption [mg]
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|