Petromont HDPE 1000

 

Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer

Key Words: Pharmaceutical grade, containers, packaging

Material Notes:
Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to produce containers up to 10 litres for use in various packaging applications. Petromont HDPE 1000 offers both excellent processing characteristics and finish product performance.

Petromont HDPE 1000, because of its high density, exhibits excellent rigidity and top load performance while still offering outstanding drop impact properties, as well as maintaining excellent environmental stress crack resistance performance. The higher density also makes this product a good candidate for some hot filled applications. The glossy appearance, which is characteristic of Pétromont’s resins, results in parts exhibiting good surface quality. The highly stabilized additive package makes Petromont HDPE 1000 less susceptible to degradation during processing. In regards to swell characteristics, Petromont HDPE 1000 is similar to most competitive resins having similar viscosity properties.

Available Properties
  • Density
  • ESCR 100% Igepal®
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • CTE, linear 20°C
  • Melting Point
  • Crystallization Temperature
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。