Petromont HDPE 2001

 

Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Film

Key Words: Film

Material Notes:
Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion and millinery bags, food packaging, "T-shirt" bags, industrial and agricultural bags, etc.

Petromont HDPE 2001 has a broad molecular weight distribution. This, combined with its high molecular weight and balanced density, results in excellent performance at high extrusion rates with high film strength and rigidity. The excellent draw down characteristics permit production of high quality thin films. This product consists of an improved formulation.

Available Properties
  • Density
  • Melt Flow
  • Melting Point
  • Vicat Softening Point
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。