Petromont HDPE 2200

 

Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Film

Key Words: Film extrusion, barrier properties

Material Notes:
Pétromont HDPE 2200 is a high-density polyethylene homopolymer resin produced using the UNIPOL® Process. This resin can be used in a mono layer or co-extrusion resin in applications requiring improved film stiffness and barrier properties, such as in Deli Wrap, cereal box liner, etc.

Pétromont HDPE 2200 is an intermediate molecular weight resin offering an excellent combination of maximum barrier properties and stiffness with no detectable taste and odour as well as good extrusion characteristics.

Available Properties
  • Density
  • Water Vapor Transmission
  • Oxygen Transmission
  • Nitrogen Transmission
  • Carbon Dioxide Transmission
  • Melt Flow
  • Melting Point
  • Crystallization Temperature
  • Vicat Softening Point
  • Process
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。