Petromont HDPE 3000
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Injection Molding
Key Words: Food grade, crates, cases, trays
Material Notes: Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and other similar objects requiring rigidity, toughness and freedom from warpage.Petromont HDPE 3000 is a medium molecular weight homopolymer resin. Its very narrow molecular weight distribution and high density make it ideally suited for injection moulding applications where outstanding stiffness, warp resistance and toughness are demanded. Parts moulded from Petromont HDPE 3000 exhibit high gloss, low odour and are suitable for food packaging applications.
| Available Properties |
- Density
- ESCR 10% Igepal®
- Melt Flow
- Tensile Strength, Yield
- Flexural Modulus
- Tensile Impact Strength
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|