Haveg 41NA Phenolic; Silicate Filled
Subcategory: Phenolic; Thermoset; Polymer
Key Words: Ametek-Haveg Division; Haveg Phenolic
Material Notes: A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers.
| Available Properties |
- Density
- Hardness, Barcol
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|