Resinoid 7051 Phenolic Molding, Glass Reinforced
  Subcategory: Phenolic; Thermoset; Polymer 
Close Analogs: 27 Resinoid phenolic molding compounds are listed in MatWeb.  Type 'Resinoid' in the text search box to view them. 
Material Notes:  Data provided by the manufacturer. The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance 
  
  
    | Available Properties | 
   
    
    - Density
 
- Water Absorption
 
- Linear Mold Shrinkage
 
- Hardness, Rockwell E
 
- Hardness, Rockwell M
 
- Tensile Strength, Ultimate
 
- Flexural Modulus
 
- Flexural Yield Strength
 
- Compressive Yield Strength
 
- Izod Impact, Notched
 
- Dielectric Strength
 
- Arc Resistance
 
- Comparative Tracking Index
 
- Hot Wire Ignition, HWI
 
- High Amp Arc Ignition, HAI
 
- High Voltage Arc-Tracking Rate, HVTR
 
- CTE, linear 20°C
 
- Maximum Service Temperature, Air
 
- Deflection Temperature at 1.8 MPa (264 psi)
 
- UL RTI, Electrical
 
- UL RTI, Mechanical with Impact
 
- UL RTI, Mechanical without Impact
 
- Mold Temperature
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |