Resinoid 2016 Phenolic Molding, Fabric Reinforced
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: 27 Resinoid phenolic molding compounds are listed in MatWeb. Type 'Resinoid' in the text search box to view them.
Material Notes: Data provided by the manufacturer. The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|