Pinnacle Polymers 1508 Polypropylene Homopolymer, Fiber Spinning Grade
Subcategory: Polypropylene; Thermoplastic
Material Notes: This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency. Features: - Excellent resistance to UV degradation
- Superior fiber spinning characteristics
- Resistance to gas fading
- Enhanced fiber resiliency
- Excellent lot-to-lot consistency
Applications: - Fiber spinning
- Critical extrusion applications
Certifications: Pinnacle's polypropylene, as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 (c) 1.1a entitled "Olefin Polymers" of the Food Additives Amendment of 1958 to the United States Food, Druf and Cosmetic Act of 1938. This product is permitted by the FDA for use in food-contact applications under conditions of use B through H of Table 2 in Title 21, CFR Part 176.170 (c) Information provided by Pinnacle Polymers.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|