Plaskolite Optix® PL-52 Acrylic Resin
Subcategory: Acrylic; Thermoplastic; Polymer
Key Words: PMMA; Polymethyl Methacrylate
Material Notes: Injection/extrusion pellets. High heat resistance/medium flow. Data provided by the manufacturer, Plaskolite, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Refractive Index
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|