Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Subcategory: Acrylic; Thermoplastic
Key Words: PMMA; Polymethyl Methacrylate
Material Notes: Continuously processed acrylic sheet. Data provided by the manufacturer, Plaskolite, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell M
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Gardner Impact
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Haze
- Transmission, Visible
|
|
|
|