Cookson Group Plaskon® SMT-B-1LV Molding Compound for PBGAs
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: This material is an epoxy molding compound designed specifically for grid arrays (BGA/LGA). Using an improved optimized filler system, it provides a lower viscosity with higher flow characteristics than SMT-B- 1. It is formulated with a unique resin system, which minimizes warpage and enables trouble-free molding onto rigid and flexible laminate substrates. Minimal dimensional change after molding, post bake and subsequent solder treatment make this compound an excellent choice for grid arrays. Features: - Improved wire sweep performance
- Low stress
- Minimal warpage
- Outstanding high temperature flexural strength
Information provided by Cookson Electronics
| Available Properties |
- Specific Gravity
- Viscosity
- Spiral Flow
- Ash
- Storage Temperature
- Hardness, Shore D
- Flexural Modulus
- Flexural Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Glass Temperature
- Flammability, UL94
- Oxygen Index
- Mold Temperature
- Back Pressure
- Cure Time
- Cure Time
- Gel Time
- Shelf Life
- Hydrolyzable Halides
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|