Cookson Group Plaskon® SMT-B-1FX Molding Compound for PBGAs

 

Subcategory: Epoxy; Adhesive; Thermoset

Material Notes:
This material is an epoxy molding compound optimized specifically for PBGA applications. It is a reduced catalyst version of SMT-B-1F and provides a 1-2% wire sweep improvement in most applications. It has the same unique resin system as the SMT-B-1, which minimizes warpage and enables trouble-free molding onto rigid and flexible laminate substrates. Minimal dimensional change after molding, post bake and subsequent solder treatment make this compound an excellent choice for PBGA applications.

Features:

  • Faster cure speed
  • Improved wire sweep performance
  • Improved warp performance
  • High HSTL performance
  • Lower viscosity
  • Reduced cure time

Information provided by Cookson Electronics

Available Properties
  • Specific Gravity
  • Viscosity
  • Spiral Flow
  • Ash
  • Storage Temperature
  • Hardness, Shore D
  • Flexural Modulus
  • Flexural Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Glass Temperature
  • Flammability, UL94
  • Oxygen Index
  • Mold Temperature
  • Back Pressure
  • Cycle Time - Injection
  • Cure Time
  • Gel Time
  • Shelf Life
  • Hydrolyzable Halides
  • Preheat Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。